Title: Effect of Mn addition on serrated plastic flow behaviour in high-strength multiphase steels with retained austenite
Authors: Kozłowska, Aleksandra
Grzegorczyk, Barbara
Staszuk, Marcin
Grajcar, Adam
Citation: JIRKOVÁ, Hana ed.; JENÍČEK, Štepán ed. Proceedings PING 2019: modern trends in material engineering: 10.-13.09.2019, Pilsen. 1. vyd. Plzeň: University of West Bohemia, 2019, s. 40. ISBN 978-80-261-0879-5.
Issue Date: 2019
Publisher: University of West Bohemia
Document type: konferenční příspěvek
conferenceObject
URI: http://hdl.handle.net/11025/35227
ISBN: 978-80-261-0879-5
Keywords: středně-manganová ocel;Portevin - Le Chatelierův jev;vliv obsahu manganu;zdokonalená vysokopevnostní ocel
Keywords in different language: medium-Mn steel;Portevin–Le Chatelier phenomenon;influence of manganese content;advanced high-strength steel
Abstract in different language: The effect of manganese addition (from 3 to 5%) on the serrated plastic flow behavior in medium manganese TRIP steels was investigated in static tensile tests performed in a temperature range of 20-200°C. The Portevin-Le Chatelier (PLC) effect was observed in a steel containing the higher Mn content. The effect of deformation temperature on the critical strain for the serrated flow was noted. The relationships between the manganese content, deformation temperature, mechanical properties and the appearance of serrated flow were characterized.
Rights: © University of West Bohemia
Appears in Collections:Proceedings PING 2019: modern trends in material engineering
Proceedings PING 2019: modern trends in material engineering

Files in This Item:
File Description SizeFormat 
Kozlowska.pdfPlný text179,39 kBAdobe PDFView/Open


Please use this identifier to cite or link to this item: http://hdl.handle.net/11025/35227

Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.